Blue Jay Gold Adds Antimony Potential at High-grade Steller Project
Original announcement by investingnews on
- Company
- Blue Jay Gold
- Ticker
- JAY
- Exchange
- Unavailable
- Region
- Yukon
- Primary commodity
- Gold
- Secondary commodities
- Silver, Antimony
- Document categories
- Drill results, Metallurgy
- Extracted
- 2026-10-23 18:48:27 UTC
Analysis by Minestarters Atlas
Atlas analysis published:
Minestarters Atlas analysis
Summary
Blue Jay Gold has reported high-grade gold and silver results from its Steller project in the Yukon, including a 14m intercept at 6.15 g/t Au and 124 g/t Ag. Additionally, preliminary metallurgical testing at the Becker-Cochran prospect yielded a high-grade antimony concentrate with 93.9% recovery.
Reasoning: The document reports a high-grade gold-silver intercept that extends previous drilling and provides promising preliminary antimony metallurgical results.
Positive factors
- high-grade gold and silver intercept
- step-out extension confirmed
- strong antimony concentrate grade and recovery
Facts used in scoring: 3

Classification and evidence
Step-Out Extensionpositive
Mineralization extended beyond the previously known limit.
Why it applies: The SC26-003 hole is described as a step out from previous drilling.
Evidence · text
“a step out of about 32 metres down plunge from previous drilling”
Mill Routeneutral
Processing via mill or concentrator (CIL, CIP, tank leach, flotation).
Why it applies: the document describes a flotation route ("concentrate")
Gravity Routeneutral
Gravity separation forms a material part of the flowsheet.
Why it applies: the document describes a gravity route ("spiral")
Single Domain Onlynegative
Testing limited to one composite or domain — representativeness not established.
Why it applies: only one composite was tested
Extracted facts
Stored fact records: 3. Some facts used in scoring do not have a stored record.
Drill Results (2)
SC26-003Steller · goldGrade: 6.15Grade Unit: g/tIntercept: 14 mView all detailsHide details
Identity
- Hole ID
- SC26-003
- Project
- Steller
- Commodity
- gold
- Region
- canada_yt
- Reported Region
- canada_yt
- Ticker
- JAY
Geometry
- Grade
- 6.15
- Grade Unit
- g/t
- Intercept
- 14 m
Classification
- Program
- exploration
- Sample Type
- drill
- Group ID
- SC26-003:unknown-unknown
Location
- Location
- Skukum Creek
- Loc. Source
- document
QA/QC
- QA/QC Disclosed
- Yes
- QA/QC Methods
- duplicates
Review
- Needs Review
- No
- Interp. Status
- scored
- Historical
- No
Dates
- Event date
- 2026-10-23T00:00:00.000Z
Reasoning: 6.15 g/t Au over 14m is a strong intercept and represents a step-out from previous drilling.
Positive factors
- high grade
- step-out extension
Evidence · text
“hole SC26-003 at Skukum Creek intersected 14 meters of 6.15 grams per tonne (g/t) gold”
Tags used in scoring
QA/QC Disclosedpositive
Release includes QA/QC disclosure — certified lab, QP sign-off, or stated methods (blanks, standards, duplicates).
Why it applies: qaqc_disclosed is true
Cut-off Undisclosednegative
High-grade interval reported without stating the cut-off grade used for compositing.
Why it applies: no cutoff_grade was stated
SC26-003Steller · silverGrade: 124Grade Unit: g/tIntercept: 14 mView all detailsHide details
Identity
- Hole ID
- SC26-003
- Project
- Steller
- Commodity
- silver
- Region
- canada_yt
- Reported Region
- canada_yt
- Ticker
- JAY
Geometry
- Grade
- 124
- Grade Unit
- g/t
- Intercept
- 14 m
Classification
- Program
- exploration
- Sample Type
- drill
- Group ID
- SC26-003:unknown-unknown
Location
- Location
- Skukum Creek
- Loc. Source
- document
QA/QC
- QA/QC Disclosed
- Yes
- QA/QC Methods
- duplicates
Review
- Needs Review
- No
- Interp. Status
- scored
- Historical
- No
Dates
- Event date
- 2026-10-23T00:00:00.000Z
Reasoning: Significant silver grade accompanying the gold intercept.
Positive factors
- high grade silver
Evidence · text
“124 g/t silver”
Tags used in scoring
QA/QC Disclosedpositive
Release includes QA/QC disclosure — certified lab, QP sign-off, or stated methods (blanks, standards, duplicates).
Why it applies: qaqc_disclosed is true
Cut-off Undisclosednegative
High-grade interval reported without stating the cut-off grade used for compositing.
Why it applies: no cutoff_grade was stated
Metallurgical Results (1)
metallurgical testingSteller · antimonyRecovery: 93.9 %View all detailsHide details
Identity
- Project
- Steller
- Commodity
- antimony
- Region
- canada_yt
- Reported Region
- Yukon
- Ticker
- JAY
Test Work
- Program Status
- preliminary
- Test Type
- metallurgical testing
- Sample
- Becker-Cochran prospect preliminary metallurgical testing
Recovery
- Recovery
- 93.9 %
- Conc. Grade
- 66.9
- Conc. Grade Unit
- %
Review
- Needs Review
- No
- Historical
- No
Dates
- Event date
- 2026-10-23T00:00:00.000Z
Reasoning: 93.9% recovery and 66.9% Sb grade are strong preliminary results for the prospect.
Positive factors
- high concentrate grade
- high recovery
Evidence · text
“preliminary metallurgical testing produced a concentrate grading 66.9 percent antimony at 93.9 percent recovery”
How Atlas produces this analysis
Minestarters Atlas uses automated extraction to summarize mining announcements, identify reported measurements, and classify supporting evidence. Sentiment reflects the extracted narrative and classification rules; it is an interpretation, not a reported measurement. Evidence quotes and context are provided where available. Missing data, low-confidence results, and review flags indicate limitations. Check the original publisher announcement before relying on an interpretation.